Westward 20AP68 MIG Welding Wire 0.030" ER80S-D2 11 lb
Low-alloy steel MIG wire, 0.030 in diameter, ER80S-D2 classification, 80 ksi tensile strength, 11 lb plastic spool
- Low-alloy steel wire matches ASTM A182, A217, A234, A335, A336 grades
- 80 ksi tensile strength handles demanding structural joints
- 68 ksi yield strength resists deformation under load
- 030" diameter feeds smoothly through MIG guns
- 11 lb plastic spool supports extended production runs
0.030 in ER80S-D2 11 lb Spool
Westward 20AP68 is an 11 lb spool of MIG welding wire classified AWS ER80S-D2 with a 0.030 in diameter. The low-alloy steel wire delivers 80 ksi tensile strength and 68 ksi yield strength as welded. It runs on DCEP current and ships on a plastic spool for MIG (GMAW) processes.
Low-alloy steel structural and pipe welds
This wire suits fabricators joining ASTM A182, A217, A234, A335 and A336 grade low-alloy steels where the design calls for 80 ksi tensile and 68 ksi yield minimums. It is not for jobs that specify a different AWS classification, a larger or smaller wire diameter, or a non-low-alloy base metal.
AWS ER80S-D2 classification with 80 ksi tensile
The decisive spec is the AWS ER80S-D2 classification, which guarantees 80 ksi tensile strength and 68 ksi yield strength on the listed ASTM grades. If your procedure requires a different classification or strength level, this wire will not meet code.
Highlights
- Low-alloy steel wire matches ASTM A182, A217, A234, A335, A336 grades
- 80 ksi tensile strength handles demanding structural joints
- 68 ksi yield strength resists deformation under load
- 030" diameter feeds smoothly through MIG guns
- 11 lb plastic spool supports extended production runs
Specifications
| Brand | WESTWARD |
|---|
Questions about this item
What wire diameter and spool weight does the 0.030" ER80S-D2 spool use?
The spool contains 11 lb of 0.030 in diameter ER80S-D2 low-alloy steel wire on a plastic spool.
Which polarity and AWS classification are required for this MIG wire?
The wire is classified AWS ER80S-D2 and must be run with DCEP polarity for MIG (GMAW) welding.
What tensile strength does the as-welded deposit provide and when should the spool be replaced?
The as-welded deposit delivers 80 ksi tensile strength; replace the spool when the 11 lb of wire is consumed or if the wire shows rust or damage.