Value Brand
Value Brand 41R176 14 in Stick Electrode 3/32 in AWS ENiFe-Cl 1 lb
A 14-inch cast-iron stick electrode, 3/32-inch diameter, AWS ENiFe-Cl classification, 58 ksi minimum tensile strength, DCEP current
- TypeWelding Supplies
- NiFe-Cl classification suits cast-iron repairs
- 14 in length gives good reach in tight joints
- 3/32 in diameter fits standard SMAW holders
- 58 ksi minimum tensile meets AWS strength requirement
- 1 lb pack keeps consumable stock manageable
Cast Iron Stick Electrode 14 in 3/32 in
The WESTWARD 41R176 stick electrode is classified AWS ENiFe-Cl for cast iron welding. It measures 14 in overall length with a 3/32 in diameter and weighs 1 lb. Minimum tensile strength is 58 ksi with as-welded tensile strength of 58 to 84 ksi.
Suitable for Cast Iron to Carbon Steel Joints
This electrode suits repair or fabrication joining cast iron to carbon steel or cast iron to cast iron using DCEP current. It is not for buyers who need a different AWS classification or a larger diameter for higher deposition rates.
AWS ENiFe-Cl Classification Decides Fit
The single specification that decides whether this is the right part is the AWS ENiFe-Cl classification, which defines the electrode chemistry and mechanical properties for cast iron applications.
Highlights
- NiFe-Cl classification suits cast-iron repairs
- 14 in length gives good reach in tight joints
- 3/32 in diameter fits standard SMAW holders
- 58 ksi minimum tensile meets AWS strength requirement
- 1 lb pack keeps consumable stock manageable
Specifications
| Brand | WESTWARD |
|---|---|
| Type | Welding Supplies |
Questions about this item
How do I install the 14 in ENiFe-Cl electrode in my stick welder and what step is often missed?
Clamp the 3/32 in electrode in the holder, set the machine to DCEP polarity, and clean the cast iron joint thoroughly before welding — the preparation step many users skip.
What maintenance or replacement will the 1 lb pack of ENiFe-Cl electrodes need later?
The electrodes are consumable; each 14 in rod is used until it burns down to the stub, then you replace it with a fresh one from the pack.
What limit appears first when running the ENiFe-Cl electrode continuously on cast iron?
The electrode reaches its 58 to 84 ksi tensile strength range as-welded; exceeding the recommended amperage for the 3/32 in diameter causes overheating and porosity first.